Before the classes started I did some moulds, but, happened that it was not working so well because after three times use the mould started to beak. In addition, I was taking too much time to retouch each piece. Therefore, the production was definitely not efficient. In conclusion, I was needing to do better moulds with a better plaster.

The red clay was not working very well also, my kitchen was all red, my clothes, my shoes, my carpet, pretty much everything turned red.

After I bought a proper dentist plaster, witch is harder than the normal one, my set of moulds started to work properly.
I also brought a new clay, it can be firing at 1000 C, so, it wont shrink too much, probably the same as the red clay shrinks.